[MW:20389] Requirment of Hardness Test for PQR of SB 575 UNS N06059.

 
Dear All,
 
While performing a PQR of butt joint (plate to plate ) of SB 575 UNS N06059 to SB 575 UNS N06059 with ASME sec IX ,
Is it a hardness test is required ? ( except tension & bend ).
Is this hardness requirement is requirement of other code like Sec II part B?
 
plz guide.
 
Ganesh Mahankal
Alfa Laval India Ltd Pune India
+91 9970357971
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...