S355J2 the impact is done at -20 and S355K2 is -40


On Saturday, 26 October 2013, 20:56, hany alfy <hanyon_alfy@yahoo.com> wrote:
Dear All

ASTM A 514  is grade of plates which used for Mechanical Cripple
can anyone suggest any equivalent grade for it?

Regards,
H.A 


On Wednesday, February 2, 2011 12:34 PM, Karthik <karthik6684@yahoo.com> wrote:
http://www.splav.kharkov.com/steelgrade/mat_start_eu.php?name_id=10#1

or

http://www.arcelormittal.com/fce/prd_web/new_web_details.pl?code=A30&langlist=EN



Equivalent grades of grade   S355J2 (1.0577)
USA
-
Germany
DIN,WNr
Japan
JIS
European old
EN
China
GB
Sweden
SS
A656
St52-3N
SS490YA
Fe510D2
S355J2G4
Q345D
2134-01


Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Wed, 2/2/11, bujji <chakri.cruise@gmail.com> wrote:

From: bujji <chakri.cruise@gmail.com>
Subject: [MW:9676] details of equivalent materials list
To: materials-welding@googlegroups.com
Date: Wednesday, February 2, 2011, 2:51 PM

Hi All,
         can anyone give me the details of equivalent materials list ?
 
For eg : S355k2+N is EH-36 (40 MM plates)
 
 
S355 J2 is equivalent to ----------- ??? (round bar dia  70 mm)
 
 
Regards,
chakri.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...