Thursday, October 24, 2013

RE: [MW:19070] RE: 19048] Mode of Metal transfer for GMAW

Pradip,
 
There is one particular mode of transfer, GMAW-STT This may be considered as a SC Mode also
 
Regards,
 

Subject: [MW:19056] RE: 19048] Mode of Metal transfer for GMAW
Date: Wed, 23 Oct 2013 16:32:02 -0500
From: jhenning@deltak.com
To: materials-welding@googlegroups.com

GMAW –

·         Short circuiting arc transfer

·         Globular transfer

·         Spray transfer

·         Pulsed arc transfer

 

For more general information see AWS Welding Handbook, volume 2, Welding Processes, Chapter 4 – metal transfer mechanisms starting on page 112.  Selection of transfer mode is usually determined on the basis of material thickness.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Pradip Ghosh
Sent: Tuesday, October 22, 2013 11:39 PM
To: materials-welding@googlegroups.com
Subject: [MW:19048] Mode of Metal transfer for GMAW

 

Dear Expert,

 

Can any one tell me that what are the metal transfer mode available for GMAW and what type of metal transfer is suitable for down hand bottom fillet welding in MAG/GMAW

 

 

Pradip Ghosh

 

QA/QC Engineer

 

Mott Mac Donald 

 

 

 

 

 

 

 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...