Wednesday, October 23, 2013

[MW:19054] Welding between Alloy 625 to P 91 and Alloy 625 to SS 347 H

My Dear Experts,
 
I need weld  SS 347 H to Alloy 625 and  also Alloy 625 to P 91 materails.  The scope of work is attached.  The follwing tests need to be done.  If any body is having expreience please share the welding  procedures of any reserch papers related to it.

a.   M icro hardness at surface and subsurface of HAZ (towards P91 side)

b.    SEM/EDS to find ferrite formation at interface (towards P91 side)

c.     Creep assessment for 1000hrs at temperature 530deg.C ( As per ASTM E139).

d.    Mechanical test

e.     Metallographic examination on cross section (to cover base metal, interface & HAZ towards P91 Side and weld)

f.     Impact Testing

g.    Chemical analysis of weld metal.

Note : Point No. b & c shall be lab report review only.

B. The Furnace PWHT shall be performed for Spool

 

 
Regards
 
VENKAT

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...