[MW:18980] Corrosion in trunnion supports of pipework containing hazardous substances

Health and Safety Executive - Safety notice

Department Name:

Hazardous Installations Directorate - CEMHD

Bulletin No:

HID1-2013

Issue Date:

8 October 2013

Target Audience:

All operators of major accident hazard plant

Key Issues:

This safety notice describes the dangers of undetected corrosion in trunnion supports of pipework containing hazardous substances, in particular tubular trunnions fitted with an end cap, and the precautions necessary to ensure continued safe operation.

Introduction:

This safety notice describes the dangers of undetected corrosion in trunnion supports of pipework containing hazardous substances, in particular tubular trunnions fitted with an end cap, and the precautions necessary to ensure continued safe operation.

Background:

Figure 1: Pipe support trunnions, open and closed end

Pipework support trunnions are common in petrochemical installations, where short lengths of tube are welded to process pipework as a means of supporting from structural steel. Various configurations are shown in Figure 1.

A release of Liquefied Petroleum Gas (LPG) occurred on a UK refinery during processing, leading to a controlled shutdown and isolation of the associated vessel and pipework. Further investigation revealed that corrosion had occurred within the trunnion supports for the pipework, with a gradual loss of wall thickness on the LPG pipe.

Figure 2: Partial cross section of closed end trunnion

The tubular support had been fitted with an end cap, forming a closed end, which in theory eliminated moisture ingress, but the trunnion also had a weep hole drilled on the underside to allow for venting. This hole was sited directly on support steelwork. As a result, the void within the trunnion gradually drew in moisture, which then condensed on the pipe wall. This in turn led to accelerated localised corrosion of the pipe. As this corrosion mechanism was not anticipated, it remained undetected until the pipe wall eventually ruptured under internal pressure. The arrangement is represented in Figure 2.

Figure 3: Radiograph of corroded pipework at trunnion

The company have conducted further investigations on site, and have found other instances of the same corrosion. This has led to immediate replacement in some cases. In total, almost 5% of the site population of trunnions has had to have some remedial work. An example radiograph of the corrosion found is shown in Figure 3.

Action required:

Operators of plant with pipework containing hazardous substances should ensure that their inspection regime includes suitable examination of supports. In particular, where tubular trunnions are installed with an end cap that prevents visual examination, other means should be employed to ensure the integrity of the system where there is a possibility of moisture ingress. Note that permanent removal of the end cap is not recommended without further design work, as the cap may be required for additional stiffness.

General note:

Please pass this information to a colleague who may have this product/equipment or operate this type of system/process.

http://www.hse.gov.uk/safetybulletins/trunnion-supports-corrosion.htm?goback=%2Egde_4439477_member_5795589142431682563%2Egmp_4439477%2Egde_4439477_member_5794392283516252164#%21

 

 


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...