Thursday, August 1, 2013

Re: [MW:18322] Welder re-qualification.

Hi Manju ,

In the PQR that you have qualified in 1G position using welder A only by SMAW process ( for Example ) of 40mm, 

if PQR passes, then the welder A is also qualified to weld unlimited thk, then why are you requalifying again .

If you want to requalify the same welder A due to some reasons, may be to test his skills, then U can use the same WPS for reference Document, for the welder qualification.

But U did not informed , how many process actually were used in PQR, what are the weld deposit Thk incase if U used 2 different welding process ?

Regards,
Saravanan






On Thu, Aug 1, 2013 at 12:14 PM, manjunath madiwalar <mmkabanur@gmail.com> wrote:
Dear Sarvan,
 
      Its IG position,  My querry is wheather can i use same  WPS to  re qualify same welder in 25mm thk plate. Welding is SMAW. 
regards.
Manjunath


On Tue, Jul 30, 2013 at 4:38 AM, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Hi Manjunath ,

If you have qualified 40mm Plate of SA 516 Gr.70, the welder who welds the PQR also qualified, as per ASME-IX.  How many welders did U use for that PQR ? What are the welding process and what are the weldmetal deposit thk. for each process, 

But the position you have mentioned is wrong, cannot be 6G for a plate .

Cheers ,
Saravanan



On Mon, Jul 29, 2013 at 7:37 PM, manjunath madiwalar <mmkabanur@gmail.com> wrote:
Dear experts.
 
       Can you give clearity.
 
   6 months back we are established  wps of  welder for 6G of 40mmthk SA516 Gr70 plate i,e qualified for range of 80mm metal thickness.. but now i want requlify welder range of  50mm maximum metal thickenss  to be weld
 
Question 1) can i use same  wps to re qualify  same welder.
                2)can i use same PQR 25mmplate sothat i can  weld upto50mm thk.
 
  i have constraint  that i do not have 40mm 516 Gr70 plate, i have 25mm thk SA516 plate.
 
  Please  suggest best option.
 
Regards.
 
Manjunath T Madiwalar. 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone