Dear Sarvan,
Its IG position, My querry is wheather can i use same WPS to re qualify same welder in 25mm thk plate. Welding is SMAW.
regards.
Manjunath
On Tue, Jul 30, 2013 at 4:38 AM, Saravanan Sornam <saravanshyla@gmail.com> wrote:
Hi Manjunath ,If you have qualified 40mm Plate of SA 516 Gr.70, the welder who welds the PQR also qualified, as per ASME-IX. How many welders did U use for that PQR ? What are the welding process and what are the weldmetal deposit thk. for each process,But the position you have mentioned is wrong, cannot be 6G for a plate .Cheers ,Saravanan--On Mon, Jul 29, 2013 at 7:37 PM, manjunath madiwalar <mmkabanur@gmail.com> wrote:--Dear experts.Can you give clearity.6 months back we are established wps of welder for 6G of 40mmthk SA516 Gr70 plate i,e qualified for range of 80mm metal thickness.. but now i want requlify welder range of 50mm maximum metal thickenss to be weldQuestion 1) can i use same wps to re qualify same welder.2)can i use same PQR 25mmplate sothat i can weld upto50mm thk.i have constraint that i do not have 40mm 516 Gr70 plate, i have 25mm thk SA516 plate.Please suggest best option.Regards.Manjunath T Madiwalar.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments