Skip to main content

Re: [MW:18500] Re : Essential Variables for Machine Welding

Hi,
Find below the ASME-IX Interpretation. Hope it will clear your doubts.

"direct visual control" - welding operator having direct visual control and giving verbal command to the welding operator having remote control.

"remote visual control" - welding operator having remote control and follow the verbal commands from welding operator having direct visual control with the weldment.

Interpretation: IX-95-31
Subject:            QW-361.2, Essential Variables – Machine Welding
Date Issued:     May 30, 1996
File No:            96-141
 
Background:  A welding operator has direct visual contact with a pipe weldment that is being welded utilizing machine orbital pipe welding equipment.  This welding operator is giving verbal commands to a second welding operator, who does not have eye contact with the weldment, and who is positioning the weld head and wire aimers located on the head remotely, during the welding of the joint in accordance with the verbal commands of the first operator.  Each welding operator has been qualified to perform both remote and direct visual control welding.
 
Question:  Are these welders qualified to make the subject weld in accordance with QW-361.2, even though the welding operator having direct visual control is directing the positioning of the orbital pipe welding equipment verbally and does not have "hands-on" control of the welding head?
 
Reply:  Yes.
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


From: mustaffi <mustaffi@dynac.com.my>
To: materials-welding@googlegroups.com
Sent: Thursday, August 22, 2013 3:38 PM
Subject: [MW:18499] Re : Essential Variables for Machine Welding

Dear All,
 
Can anybody help me to explain  in details of these statement .
 
QW 361.2 (b) Essential Variables for Machine Welding
A change from direct visual control to remote visual control
 
What's the meaning for "direct visual control"  and "remote visual control"
 
Under Page 58 – Asme Section IX 2011a
 
Best  Regards
Mus
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...