[MW:18442] Re: production test coupon requiorement as per ASME SEC VIII DIV 1

Dear all,

1. Flange Long. seam joint required PTC or not.
2. PTC required for category C & D joints.
please give a code reference for above two points.

Regards
Paul

On Friday, November 26, 2010 4:30:01 PM UTC+5:30, asad azmi wrote:
Dear all,
 
Greetings.
 
Please inform me PTC(Production test coupon requirement) for below details--
 
Construction Code :  ASME SEC VIII DIV 1
 
Shell Material :   SA 387 GR 12 CL 2,  65 & 70 Thk.
 
MDMT :  0 Deg Celcius
 
Impact test is required as per  ASME SEC VIII DIV 1.
 
The Heat number for shell material for 3 vessels is not same.
 
 
3 vessels are required to be fabricated as per the above requirement for single  client. The vessels are going to to be erected at one location only. 
 
The thichkness of shell material for 1 vessel is 65 Thk and for other 2 vessels is 70 Thk. Diameter and Length of the vessel is different. Only MDMT and material is same.
 
Please inform me whether seprate  PTC( production test coupon)  is required for each  vessel  OR 1 PTC attached with longseam/Circ. Seam of only 1 vessel  will also represent other 2 vessels also.
 
Whether 2 PTC ( 1 for longseam &  1 for circumferential seam for 1 vessel)  is enough for all three vessels OR total of 6 PTC are required for 3 vessels.
 
Please give code reference.
 
Thanks in advance for your valuable suggestions.
 
Regards
 
Asad Azmi
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...