Dear Experts,
As per B31.3 / Fig 323.2.2A Note 1: Any carbon steel material may be used to a minimum temperature of −29°C (−20°F) for Category D Fluid Service.
This means that the case ( as mentioned) not required impact test. Is this correct ?
Thanks/
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Monday, May 06, 2013 6:35 PM
To: materials-welding@googlegroups.com
Subject: [MW:17607] RE: 17605] Impact test for A106
Hello PVT,
Usually A/SA 106 is not a reliable material for design temperature below -20 DegC. If the use of C-Mn steel is insisted A/SA -333 Gr-6 would be the choice. By definition , materials falling under this specification( A/SA-333 ) are meant for low- temperature applications.
If the lowest design temperature is -150 DegC( as mentioned below), then the choice should be austenitic S.S grades, 304L or 316L by default.
Thanks
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PVT
Sent: Monday, May 06, 2013 6:19 AM
To: materials-welding@googlegroups.com
Subject: [MW:17605] Impact test for A106
Dear Experts,
Process piping with material A106- thickness = 35 mm, design temp: 0 - 150 °C . My question: As per ASME B31.3, impact test for weld joint is required or not? If required, what temperature to impact test?
Thanks!
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment