Dear Pradip,

The reference is very clear. "MAY BE" and hence require Client/Design Engineer acceptance prior to testing.

Regards
Vino-Doha

On Sat, Nov 17, 2012 at 8:35 AM, pradip kumar sil <pradipsil@gmail.com> wrote:
Dear Everyboby,
As per ASME B-31.3 para 345.3.1 says  "All joints may be primed &
painted prior to leak testing unless a sensitive leak test (para.
345.8) is required.
But as per ASME SEC V Shows leak test  comes under :
The specific test method(s) or technique(s) and Glossary of terms of
the method in this article are describe in mandatory appendices I
through X & non mandatory appendix A as follows:
Appendix I—Bubble Test—Direct Pressure Technique
Appendix II—Bubble Test—Vacuum Box Technique
Appendix III — Halogen Diode Detector Probe Test
Appendix IV — Helium Mass Spectrometer Test —
Detector Probe Technique
Appendix V — Helium Mass Spectrometer Test —
Tracer Probe Technique
Appendix VI — Pressure Change Test
Appendix VII — Glossary of Terms
Appendix VIII — Thermal Conductivity Detector
Probe Test
Appendix IX — Helium Mass Spectrometer Test —
Hood Technique
Appendix X — Ultrasonic Leak Detector Test
My question is HYDROTEST & PHENEUMATIC test   is comes under leak test
as per ASME B-31.3 para 435.3.1.  Can we  paint the spool joint before
hydrotest.
 Any referances for hydrotest/phenumatic test comes under leak test.
Regards
Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...