Re: [MW:15934] WQT without WPS

Mr. Srinu,

Take up the matter with your client Make a fresh WPS & PQR and it is generally accepted.

Make sure that, the PQR is successfully done and this may be acceptable to your client.

sridhar.


From: srinu p <sree.dream6@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 14 November 2012 3:35 PM
Subject: [MW:15929] WQT without WPS

Dear all,
 
My contractor doing welding without approved WPS. Now they are completed welding around 50 tanks (Under Ground Storage Tanks) out of 100 no.s. 
 
Now the client is asking WPS, is there any way to solve this problem.
 
Regards 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...