Wednesday, November 14, 2012

Re: [MW:15930] WQT without WPS

Hi


If you use ASME there are some standart WPSs in appendix E. If contractor says ok they can use it. If you use EN there are some standart WPSs also.




2012/11/14 srinu p <sree.dream6@gmail.com>
Dear all,
 
My contractor doing welding without approved WPS. Now they are completed welding around 50 tanks (Under Ground Storage Tanks) out of 100 no.s. 
 
Now the client is asking WPS, is there any way to solve this problem.
 
Regards 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--

Tuğrulhan ÖZDEMİR

Metalürji & Malzeme Müh. (Y.T.U.)

U.Kaynak Mühendisi (I.W.E.)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...