Hi, Mr Hedge,
 
Thank  you very much for your response. It was very helpful!
 
Regards,

Guttemberg
 

Em 10/11/2012 09:51, Prakash Hegde < pb.hegde@yahoo.com > escreveu:
Hi! Friends
Attached inforamtion may be helpful to you
 
Regards
 
Hegde P.B.
Welding consultant Pune
+918805593046

--- On Fri, 9/11/12, Guttemberg <guttemberg.souza@uol.com.br> wrote:

From: Guttemberg <guttemberg.souza@uol.com.br>
Subject: [MW:15877] Enc.: 15825] PWHT -9%Cr-1%Mo/V materials
To: materials-welding@googlegroups.com
Date: Friday, 9 November, 2012, 3:56 AM

 
 
Conectado pela Motorola


-------- Mensagem original --------
Assunto: Re: 15825] PWHT -9%Cr-1%Mo/V materials
De: Guttemberg <guttemberg.souza@uol.com.br>
Para: pgoswami <pgoswami@quickclic.net>
Cc:

Dear Pradip,
 
Thank you very much for your aswer!
In fact we have to check the hardness values after PWHT but how many repairs are allowed to do or how many cycles do i have to consider in the WPS qualification as per the metallurgy of these materials?
Greetings,
Guttemberg
 
Conectado pela Motorola
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...