Tuesday, November 13, 2012

Re: [MW:15919] Selection of Heat Input During Welding

Dear Mr Nandesh,

First of all thanks for your reply. As you have referred to Table 8-1 of API RP 582 - 2001: its regarding the interpass temperature which is not a variable of Heat-Input rather than affect the heatinput.

Could you give me the reference of code or standard of The ideal heat input for commonly used welding processes lies in between 0.8 kJ/mm to 2 kJ/mm.

Yes, heatinput range always supposed to mention in WPS but i need to make it.



On Mon, Nov 12, 2012 at 3:27 PM, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:

Heat input is not a thing that you can select, rather to be controlled by means of welding Voltage, current, travel speed, electrode diameter etc.

The ideal heat input for commonly used welding processes lies in between 0.8 kJ/mm to 2 kJ/mm. The heat input that you can be used during the production welding will be  "as qualified with + or - some % variation mentioned in your PQR"

On the other hand, the interpass temperature, which should not be more than that the applicable code restricts.

Refer Table 8-1 of API RP 582 - 2001 : Welding Guidelines for the Chemical, Oil, and Gas Industries, for recommended interpass temperature of various materials.


ವಂದನೆಗಳೊಂದಿಗೆ / Best regard
s,


Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


From: Khandaker Imamul Hasan <kimamulhasan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, 12 November 2012 11:07 AM
Subject: [MW:15912] Selection of Heat Input During Welding

Dear Expert,

Good Morning
1.       Could anybody tell me what should be the Heat Input (kJ/mm), during Welding, for the following material Carbon Steel (e.g. ASTM A-106 Gr-B), Low Alloy Steel (e.g. A335 P11, P22), Stainless Steel (e.g. A312 Tp 304L, 308L, 316L, 321)?
2.       How to select the appropriate Heat Input for a certain material.

--
Best Regards

Khandaker Imamul Hasan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Best Regards

Khandaker Imamul Hasan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...