Dear Mr shaikh

for your project is NACE  RP 0472/ NACE MR0175 is applicable then all details are mentioned 

hope u will get that


On Fri, Nov 9, 2012 at 2:23 PM, SHEIKH <kareemunsheikh@gmail.com> wrote:

Dear experts

Hardness measurements for weld joints how many locations(0,90,180,270) required each joint and any code requirement for this.

generally code mentioned base metal, haz, weld metal not mentioned how many locations need to taken from each joint 

PLEASE ADVICE MATTER IS MOST URGENT


Thanks with regards

SHEIKH 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...