Friday, November 9, 2012

Re: [MW:15885] LPG PIPE DIA Calculation

Dear Mr.Anand,
 
The std. formula  for  find out the Hydro Static Pressure = 2* S* t / D.
 
the Pipe material S= SMYS (Specified Min.Yield Strength) and , t=wall .Thk  , D=Pipe Dia Nominal ,
 
Regards,
Akbar 
On Fri, Nov 9, 2012 at 11:53 AM, anant pandit <anant0106@gmail.com> wrote:
Dear Eeperts,

Can anybody tell the formula to calculate the low pressure LPG pipeline dia, when you know the flow & length of pipe. max pressure in pipeline 2 kg/cm2 max.

Regards,

ANANT D PANDIT
For SAFESS QUALITY MGMT PVT. LTD.
PUNE.
MOBILE NO.-: +919604348931

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...