Wednesday, November 7, 2012

Re: [MW:15869] A615/A615M Steel Rebar Welding

Raj,

As per BS 7123: 1989 (Specification for Metal Arc Welding of Steel for Concrete reinforcement), for procedure qualification, full section tensile test and macro etch tests required.

Respectfully,

Nandesh Kumar A


--- On Wed, 7/11/12, DR <rzajad@gmail.com> wrote:

From: DR <rzajad@gmail.com>
Subject: [MW:15862] A615/A615M Steel Rebar Welding
To: materials-welding@googlegroups.com
Date: Wednesday, 7 November, 2012, 4:19 AM

Dear Expert,
 
We need to weld the A615/A615M Gr60 steel rebars.
 
As per specification"Chemical composition of the reinforcement steel confirming weldable quality according to british standard" & use the approved method and material for the reinforcement welding".
 
What are the procedures and qualification to be used for the welding of stel rebars.
 
Raj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...