Thursday, November 15, 2012

[MW:15937] Re: WQT without WPS

The question that needs to be answered is - how was he allowed to weld the first tank without an approved WPS? Who was inspecting and clearing the work?

There might have been a default WPS that the same contractor was using at other similar jobs. If so, that would be a little relief.

Best of luck.

Swamy

On Wednesday, November 14, 2012 3:35:33 PM UTC+5:30, srinivas wrote:
Dear all,
 
My contractor doing welding without approved WPS. Now they are completed welding around 50 tanks (Under Ground Storage Tanks) out of 100 no.s. 
 
Now the client is asking WPS, is there any way to solve this problem.
 
Regards 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...