Monday, November 12, 2012

[MW:15913] Range qualified for welder qualification by mechanical testing( ASME BPVC Section IX)

Dear All,

Is it mentioned, where to refer the range qualified for welder qualification by mecahnical testing in ASME BPV Sec IX.

By radiography it is mentioned in QW-404.3

Thanks and Regards,

Hareesh K V


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...