Re: [MW:14966] RE: 14959] Need WPS clarification with ASME and EN

Dear Kumar,

You can use if the client specify you(Go through client Standard) the equivalent ASTM material for the BS or any other material and the equivalent material falls under your qualified material range.


On Thu, Jul 26, 2012 at 6:52 AM, nguyen anh tuan <tuanpvecc@gmail.com> wrote:

Dear Kumar

 

I think you can't use WPS  for BS material  following QW-424 ASME section 9

 

Nguyen

QA/QC

Posco

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Naresh Kumar
Sent: Thursday, July 26, 2012 12:08 AM
To: materials-welding@googlegroups.com
Subject: [MW:14959] Need WPS clarification with ASME and EN

 

Dear experts,

 

I have a doubt about WPS. Our company has WPS with ASTM material by ASME standard.

Whether this WPS can be used for the equivalent BS material or not.

 

 

Thanks & Regards,

Kumar S 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...