Hi Kumar,
 
Some inspectors can accept this WPS but some would not, because EN materials will be designated as an Unassigned materials as per ASME-IX.
 
Refer ASME-IX QW-424.1 for your knowledge.
 
Better discuss with your client.
 
Regards,
Saravanan,
S.Korea

On Thu, Jul 26, 2012 at 12:06 PM, Vinayak Kale <Vinayak_Kale@lntenc.com> wrote:

Can , provided , all essential parameters & properties shall match


Regards


Vinayak Kale
OGSP - QA & I , HC - Upstream
EPC Block , 2nd Floor , Gate No.1
Saki Vihar Rd. Powai Campus
Mumbai - 400072
Ph : + 91 022 6705 3969
(M) - 9987875309
www.larsen toubro.com



[MW:14959] Need WPS clarification with ASME and EN

Naresh Kumar   to: materials-welding@googlegroups.com
07/26/2012 08:34 AM

Sent by: materials-welding@googlegroups.com



From: Naresh Kumar <snareshkumar30@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent by: materials-welding@googlegroups.com
Please respond to materials-welding@googlegroups.com




Dear experts,

I have a doubt about WPS. Our company has WPS with ASTM material by ASME standard.
Whether this WPS can be used for the equivalent BS material or not.
 
 
Thanks & Regards,
Kumar S

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Disclaimer :This email and any files transmitted with it are intended solely for the use of the addressee(s) only and may contain confidential and/or privileged information. If you are not the addressee, then this message is not intended for you and be advised that you have received this email in error and that any use , dissemination , forwarding, printing or copying of this email is strictly prohibited. In such case please notify the sender and delete this email and any attachments with it from your system immediately.Receipt of this email by you shall not give rise to any liability on the part of Larsen & Toubro Limited

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...