Re: [MW:14922] welding & base metal hardness requirement for SA 387 Gr.5 Class II plate welding with E8018-B6

Hi!
Generaly for this grade of Steel 235 BHN max is recomended for weld , HAZ ,After PWHT and base material generaly you get 200BHN max
 
Regards
 
Hegde

--- On Sat, 21/7/12, sevak hiren <hirensevak80@gmail.com> wrote:

From: sevak hiren <hirensevak80@gmail.com>
Subject: [MW:14916] welding & base metal hardness requirement for SA 387 Gr.5 Class II plate welding with E8018-B6
To: materials-welding@googlegroups.com
Date: Saturday, 21 July, 2012, 11:27 AM

Dear Experts,
 
Can anyone provide welding & base metal hardness requirement for SA 387 Gr.5 Class II plate welding with E8018-B6.
 
Thanks & Regards
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...