Friday, July 20, 2012

Re: [MW:14912] From GTAW bare filler with Ar shield to GTAW Fux Cored filler without Ar shield

You have to prepare a new WPS and qualify the welding procedure.
Change in filler metal product form is an Essential variable as per ASME Sec.IX QW-404.23

 

QW-404.23 A change from one of the following filler

metal product forms to another:

(a) bare (solid) or metal cored

(b) flux cored

(c) flux coated solid or metal cored

(d) powder
 Is an essential variable for GTAW process.

Regards
 
Prem Nautiyal

--- On Fri, 7/20/12, Shashank Vagal <nach_sam@yahoo.com> wrote:

From: Shashank Vagal <nach_sam@yahoo.com>
Subject: [MW:14905] From GTAW bare filler with Ar shield to GTAW Fux Cored filler without Ar shield
To: materials-welding@googlegroups.com
Date: Friday, July 20, 2012, 9:50 AM

Gents,
This one is related to switch over of GTAW electrode - from a bare one requiring Ar purging + shielding to the other flux cored one not requiring purging + shielding due to inaccessibility and large / long pipe sections under welding.
We have a WPS for using ER308L - Esab which requires Ar purging and shielding. But now, due to difficulties in maintaining Ar gas inside the long sections of large dia SS 304L pipes during root pass our contractor has suggested another electrode which does not need Ar purging + shielding.

Is this switch over allowed without re-qualification?

Alternate electrode suggested is this: KOBE TGX 308L STAINLESS STEEL FLUX CORED TIG WIRE (possibly 2.2 mm dia)

Thanks,

Shashank Vagal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...