Re: [MW:14908] EN 10204 - 3.2 Certificate for Assembled product

Many people think that EN 10204 only covers the type of inspection reports.
 
But they overlook that it is only valid for metallic products/materials and the corresponding manufactures of these materials. Please read EN 10204 again and have a look on the definitions of manufacturer and material.
 
EN 10204 is only applicable for metallic products. A metallic product is not a valve / any assembled product, but - as written in EN 10204 - metal sheets, bars, forgings and castings. EN 10204 can also be used for non-metallic products but it is in any case related to raw materials only.
 
 
On Thu, Jul 19, 2012 at 9:21 AM, Shashank Vagal <nach_sam@yahoo.com> wrote:
Gents,
In case of assembled products an MDR from the manufacturer incorporating MTCs for components used can be the acceptable mode of certification.
Best regards,
Shashank Vagal

--- On Wed, 18/7/12, meisam shokri arfaei <meisamshokri@gmail.com> wrote:

From: meisam shokri arfaei <meisamshokri@gmail.com>
Subject: Re: [MW:14890] EN 10204 - 3.2 Certificate for Assembled product
To: materials-welding@googlegroups.com
Date: Wednesday, 18 July, 2012, 5:30 PM


Dear Sevak
I don't know why you think so, but basically certificate type 3.2 can be use for both row materials and assembled products. Please have a look on part 4.2 of the EN 10204-2004. There mentioned that manufacturer can uses the test results in the 3.2 certificate of his row material directly (without any new test) in the 3.2 certificate of his product.
 
Regards

On Wed, Jul 18, 2012 at 9:05 AM, sevak hiren <hirensevak80@gmail.com> wrote:
Dear Experts,
 
EN 10204 Type 3.2 Certificate is applicable to non-metalic & metalic products like plates, sheets, bars, forgings, castings etc. (Applicable to raw material products only)
 
So, this type of certificate can not be issued for complete assembled products like Valve, Pump, any machine etc.
 
Please let me know your views.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
M. Shokri Arfaei
International Welding Engineer (IWE)
ASNT NDT Level III
ERI Metallurgy Lab. Manager
Tel: +98-21-66282127
Fax: +98-21-66282779
 
Please don't print this e-mail unless you really need to. BeGreen!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...