Re: [MW:14904] welding of dissimilar material CS SA106 to SS 316

If the P Nos. are same your current WPS will suffice if all essential variables are same.

Ammar

On Thu, Jul 19, 2012 at 12:10 PM, <osikwemhepaul@gmail.com> wrote:
Hello All
You need to give more information of your essential variables, that will determine if you can use the same WPS
Regards
Paul

Sent from my iPad

On 18 Jul 2012, at 9:10 PM, Tiger <ezatadel2008@gmail.com> wrote:

Dear Exprets,
 
 i have a fillet weld of dissimilar material CS SA106 to SS 316 but i don't have WPS , also i have WPS for CS TO SS ( A333 GR6 P.1 to A312 TP316 P.8 ) if it is applicable to use it for the other material.
 
thanks,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...