Thursday, July 19, 2012

Re: [MW:14900] Diffusible Hydrogen Test of Low Hydrogen Electrode

If the diffusible H2 content  specified in the TC falls within the allowable range and acceptable no need to check in every batch.

If the TC values are questionable or if the cold/H2 cracks are noticed often in the weld or if the job is sensitive type, you can cross check the values once in a while.

But,  it is mandatory to  to re dry/bake  all the LH electrodes in the electrode drying oven prior to its use to reduce the moisture content in the coating and reduce the hydrogen level .

sridhar.


From: prem nautiyal <prem_nautiyal26@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 18 July 2012 10:33 PM
Subject: Re: [MW:14892] Diffusible Hydrogen Test of Low Hydrogen Electrode

Yes.
Every low hydrogen electrode e.g. E7018, Batch Test certificate must specify this value. Almost all the reputed consumable manufacturer's check the diffusible hydrogen and report the values in their batch TC.
Please refer Table 11 in SFA-5.1 of ASME Sec. II-C.
Also if you have specified the diffusible hydrogen content requirement in your welding consumable procurement specifications then it is mandatory for consumable manufacturer to report the values.
 
Regards
 
Prem Nautiyal
Cell: 9769316004

--- On Wed, 7/18/12, Biplab Pal <biplab.mech@googlemail.com> wrote:

From: Biplab Pal <biplab.mech@googlemail.com>
Subject: [MW:14886] Diffusible Hydrogen Test of Low Hydrogen Electrode
To: materials-welding@googlegroups.com, "chandan.majumdar" <chandan.majumdar@sgs.com>, "JALADHAR JENA" <jdjena2006@yahoo.co.in>, "pinaki boxi" <boxi.pinaki@gmail.com>
Date: Wednesday, July 18, 2012, 9:59 AM

Dear Experts,

I have a doubt,
Is it mandatory to check the diffusible hydrogen test for every batch of Low Hydrogen electrode as per sec-II part c.
Please give me the code reference.

--
Thanks & Regards
Biplab Pal
Mechanical Inspector (PMT)
YASREF Project

E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...