Sunday, July 8, 2012

Re: [MW:14807] Filler wire for pipe alloy steel (P22) to cs (P1)

Dear Bijay,

It would be better to use carbon steel consumable ER 70 S2 followed by stress relieving of joint as per applicable code of construction.

Regards
Ravinder sharma

Sent on my BlackBerry® from Vodafone

From: Bijay <bkchoudhury80@yahoo.com>
Sender: materials-welding@googlegroups.com
Date: Sun, 8 Jul 2012 03:56:53 -0700 (PDT)
To: materials-welding@googlegroups.com<materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: [MW:14805] Filler wire for pipe alloy steel (P22) to cs (P1)

Dear Experts,

Kindly suggest me which filler wire best suitable for dissimilar metal pipe joints P22 to cs SA106 Gr B

Awaiting for your valuable answer
 
With Regards

Bijay Kumar Choudhury
Mob +91 94084 43554
Mob +91 89806 30973

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...