[MW:14993] Which Electrode/Filler wire we should use for 12Cr1MoV ?

Dear Experts,
 
In Thermal Power we have material of Strape plate is 15CrMo & we are using E8018B3,
 
Now New material 12Cr1MoV is coming for structure & piping work. Can we use ER 90SB3 + E9018 B3 ?which electrode & filler wire we should use as per standard.
 
If Not kindly suggest me Which Electore & filler wire should we use, as per the standards.
 
Waiting for Reply.
 
Regards.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...