Dear expert's,
anybody can give me a calrification regarding backing & back weld
as per my knowledge ,welding with back strip,retainers or weld metal (double bevel groove) can considered as backing
single bevel groove ,welding filled from groove side then gouged from inside root and finish with one single layer or more called back weld
qustns
1) is anywhere in the code given any t limitation or how many layers can weld from inside root (single bevel groove) for back weld ? (more layers can consider as double bevel is it rit)
2) one wleder qualified in 16 mm plate single bevel groove with backing, can he weld a double bevel groove of 30mm plate or not ?
3) one welder qualified for 16 mm plate single bevel groove with backing,can he wled a single bevel groove of 8 mm plate with back weld ?
thanks in adavnce
praveen --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-