Monday, July 23, 2012

[MW:14928] brazing wire for EEMUA145&146(1987) UNS7060X

Dear Experts,
 
Pls advise the sutable Brazing wire for the material EEMU A145&146 (1987) UNS 7060X

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS