[MW:14913] Acceptance criteria of ASME SEC II Part C

Dear Experts,

Can we use EM12K (Classification F7A4-EM12K) wire with 995N (Classification F9A2-EG) Flux combination?. If we use which acceptance criteria will follow according to ASME SEC II Part C.


Regards,

PVS.Krishna

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.