Gents,
This one is related to switch over of GTAW electrode - from a bare one requiring Ar purging + shielding to the other flux cored one not requiring purging + shielding due to inaccessibility and large / long pipe sections under welding.
We have a WPS for using ER308L - Esab which requires Ar purging and shielding. But now, due to difficulties in maintaining Ar gas inside the long sections of large dia SS 304L pipes during root pass our contractor has suggested another electrode which does not need Ar purging + shielding.

Is this switch over allowed without re-qualification?

Alternate electrode suggested is this: KOBE TGX 308L STAINLESS STEEL FLUX CORED TIG WIRE (possibly 2.2 mm dia)

Thanks,

Shashank Vagal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...