Dear Sir,
Thanks for your reply.
Actually my issue is not related to welding of 410S.
What will be soaking temperature after explosion bonding i.e.cladding of SA 516 Gr 70+ SA 240 Tp 410S.
Thanks and Regards
-original message-
Subject: Re: [MW:14984] Stress relieving of 410S
From: Rejoy Thomas <rejoythomas90@gmail.com>
Date: 30-07-2012 1:17 pm
which electrode are u using for this purpose..i think it'z not
E309..if u r using E 410-XX electrode for welding, then heat to
730-760°C and hold for one hour before cooling it to ambient
temperature.. Refer SFA 5.4 Table 6..
On 7/28/12, kundan.ahirao@gmail.com <kundan.ahirao@gmail.com> wrote:
> Dear expert
> kindly advice and share your opinion
> we have cladding of SA516 gr 70 + SA 240 tp 410S.
> After explosion bonding manufacturer is giving SR cycle to clad plate at
> soaking temp 675 deg C.
> But at this temperature tensile strength of base metal will achieve or not.
> If not then what will be soaking temperature.
> Also as per our fabrication drg soaking temp given is 620 deg C.
> Thanks and regards
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...