Tuesday, June 21, 2011

Re: [MW:11415] Minimum Pipe thickness in Process piping


Dear frnd,

mimimum thickness means the thickness at which it can sustain max allowable working pressure ,( MAWP )

REGARDS

DINESH
On Tue, Jun 21, 2011 at 10:45 AM, Krishnakumar M S <krishnakumarms01@yahoo.com> wrote:

Dear All

I have a query regarding Pipe thickness for CS & SS Pipes.

 

What is the Minimum Pipe thickness provided in Process piping (ASME B31.3)

Is the min. thickness is related to "Retirement Thickness"  and

What is the significance when used in AG / UG piping.

 

could any body help me to answering on this….

 


Regards,

 

Krishnakumar.M.S

Design Engineer (Piping)

Fact Engineering & Design Organisation (FEDO)

Cochin, Kerala

INDIA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...