Monday, June 20, 2011

Re: [MW:11390] Correct Answer need

Hi,
Answer is - (b)...Justification is given below.

CARBON EQUIVALENCY
Carbon equivalency (C.E.) is used to give an overall carbon percentage to estimate the risk of cracking. The higher the carbon content; the harder the steel - the more susceptible it is to cracking.
A carbon equivalency of 0.04% and above gives a greater risk of cracking.


Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Sun, 6/19/11, Nandesh Kumar <nandeshkumar@rocketmail.com> wrote:

From: Nandesh Kumar <nandeshkumar@rocketmail.com>
Subject: Re: [MW:11385] Correct Answer need
To: materials-welding@googlegroups.com
Date: Sunday, June 19, 2011, 9:42 PM

(d)

--- On Sun, 19/6/11, javed iqbal <jvd_qbl@yahoo.com> wrote:

From: javed iqbal <jvd_qbl@yahoo.com>
Subject: [MW:11379] Correct Answer need
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Sunday, 19 June, 2011, 8:41 AM

Dear all,
Nedd answer of followin detail.
Thanks
Javed
 
   Carbon equivalent values are useful to determine:
 
(a)    Weldability aspects
(b)   Crack sensitivity aspects
(c)    Typical mechanical properties
(d)   All of the above
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...