Wednesday, June 8, 2011

Re: [MW:11284] WELDING CONSUMABLES FOR WELDING P5 & P9 MATERIAL.

Dear Shiv Kumar,
 
You can go for the following consumable with "BOHLER" brand for welding P5 (X12CrMo5) and P9 (X12CrMo9-1)
according to the various processes. I think that you are the authorised dealer of Bohler welding consumables in
Bahrain.
 
1. SMAW process = E8018-B6 = Bohler Fox CM 5 Kb
2. GTAW process = ER80S-B6 = Bohler CM 5-IG
3. GMAW process = ER80S-B6 = Bohler CM 5-IG
4. SAW process = F8PZ-EB6-B6 = Bohler CM 5-UP/BB24  
 
Thanks and Regards,
 
M.SarojKumar
India.
Mobile:+ 91 9976763705/8428093545

On Tue, Jun 7, 2011 at 1:25 PM, Shivkumar <shivkumar.g@almahroos.com> wrote:

Respected Sir,

 

I wanted to know the below following consumables for welding P5 & P9 type of materials.

 

  1. SAW PROCESS
  2. GMAW PROCESS
  3. GTAW PROCESS
  4. SMAW PROCESS

 

 

Sir, I kindly request you to reply to the needful.

 

SHIVKUMAR GHONGE.

(# 00973-39408053)

 

M.H. AL MAHROOS BSC (C)
PO BOX 65
MANAMA
KINGDOM OF BAHRAIN
PH : +973 17408090
FAX : +973 17404323.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...