Wednesday, June 8, 2011

RE: [MW:11285] COMBINATION OF 2 PQR IN ONE WPS

Hi Manoj,

Which code you refer to?

AWS D1.1 - Yes
ASME IX - No

Best regards,
Kang



Date: Tue, 7 Jun 2011 10:02:56 +0530
From: pb.hegde@yahoo.com
Subject: Re: [MW:11269] COMBINATION OF 2 PQR IN ONE WPS
To: materials-welding@googlegroups.com

Dear Manoj
Technically  in your case you can not .As in your case GTAW process is qualified for base metal up to 12mm therefore you can not use GTAW process for base metal thk more than 12 mm (Therefore generaly PQR for multiple process being qualified on the test plate having more than 38mm plate to  cover max base metal range)
Regards
Hegde P.b.


From: manoj john <manojacgnr@gmail.com>
To: materials-welding@googlegroups.com
Sent: Mon, 6 June, 2011 5:26:22 PM
Subject: [MW:11264] COMBINATION OF 2 PQR IN ONE WPS

Dear All,

I have to weld 40 mm thk ss 304 plate to be welded with root GTAW and
subsequent run by SMAW.  I have 2 WPS,one WPS GTAW + SMAW thickness
range qualified is 1.6 to 12 mm and another procedure qualified 5 mm
to 50 mm  with back gouging.

My doubt is  can i make one wps supporting with these 2 Procedure
Root with GTAW and subsequent run with SMAW so i can carry out the
welding with GTA + SMAW 40 mm thk without further procedure
qualification.

Thanks & Regards.
Manoj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...