Thursday, June 2, 2011

RE: [MW:11239] RE: 11149] Re: Reduction temperature for LTCS

When a proper and approved procedure is available for this kind of material
and there is nothing wrong with the base material I would say dismiss the
welder and find a better one.
In such case you need to cut out the weld and remove a part of base material
influenced by the welding heat and create new bevel. After that try again
with a suitable welder to weld without failures.

Met vriendelijke groeten / Best Regards

Herman Pieper

Pieper Quality Support & Inspection
Phone: +31 (0)521 380083
Fax: +31 (0)84 7539225
Cell: +31 (0)6 51691215
www.pieper-qsi.nl

-----Oorspronkelijk bericht-----
Van: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] Namens MUZAMMIL MASIH
Verzonden: woensdag 1 juni 2011 7:36
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:11230] RE: 11149] Re: Reduction temperature for LTCS

Q: if one welding joints two times came repair again one more repair
come then what will we do?

On 5/31/11, pgoswami <pgoswami@quickclic.net> wrote:
> Hello MPK,
>
> Please see the attached document ,which gives a broad overview of sour
> services both as per MR-0175(upstream) and MR-0103(downstream).Feel free
ask
> more questions if you wish.
>
> Note:-to understand sour services one does not have to be a NACE
Corrosion
> specialist. A person with good common sense and engineering background
would
> be able to comprehend the requirements after reading through the above
> documents.
>
>
> Regarding " What is reduction temperature for LTCS" if you provide the
> details about the problem, I would be able to guide you.
>
> Thanks and best regards.
>
> Pradip Goswami,P.Eng.IWE
> Welding & Metallurgical Specialist & Consultant
> Ontario,Canada.
> Email-pgoswami@sympatico.ca,
> pgoswami@quickclic.net
>
> -----Original Message-----
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Kannan
> Sent: Wednesday, May 25, 2011 12:26 PM
> To: Materials & Welding
> Subject: [MW:11149] Re: Reduction temperature for LTCS
>
> To understand Sour service you have to spend some time turning pages of
NACE
> MR 0175 all parts and MR 0103 to start with. Later on API RPs.
> After that you are sure to become a corrosion specialist, depending on
your
> understanding.
>
> I fail to understand your question "What is reduction temperature for LTCS
> ?"
>
> Kannan
>
> On May 18, 1:39 pm, mpk mpk <ranmi2...@gmail.com> wrote:
>> Dear Experts,
>>
>> What is reduction temperature for LTCS & what is sour service.
>>
>> Thank You.
>>
>> MPK..
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...