Please refer QW 462.2 and QW-160,if you are following ASME IX.
On Jun 2, 11:38 am, "Pieper QSI" <pieper-...@kpnmail.nl> wrote:
> Dear Sir,
>
> You first have to tell us which specification applies and what is the
> material thickness?
>
> Met vriendelijke groeten / Best Regards
>
> Herman Pieper
>
> Pieper Quality Support & Inspection
>
> Phone: +31 (0)521 380083
>
> Fax: +31 (0)84 7539225
>
> Cell: +31 (0)6 51691215
>
> www.pieper-qsi.nl
>
> Van: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] Namens senins welo
> Verzonden: dinsdag 31 mei 2011 15:57
> Aan: materials-welding@googlegroups.com
> Onderwerp: [MW:11225] bend test specimen size
>
> Dear experts,
>
> can u help me? what is the size for bend test specimen for plate ?
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment