Re: [MW:10875] acceptance standards for pittings for SA 516 GR 70 Plates

Dear Mr Ricardo,
 
is it acceptable if plate thickness is  within acceptable limit and piting can be left as it is.
 
is there any surface conditionong/smoothenening is required or not.
 
 
 
pls suggest and give code reference if possible.
 
thanks and regards

On Tue, Apr 26, 2011 at 4:05 PM, Dindo <dindodelacruz@gmail.com> wrote:
Hi Azmi
 
If it is for new construction, then you can check the minimum thickness, If it doesn't meet your PO or thickness requirement then you can reject the plates, the supplier should have fix the pitting on their side and done all NDE required.
 
Ricardo

On Tue, Apr 26, 2011 at 2:01 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi Azmi,
 
CA-Corrosion Allowance
 
You may refer the material spec. to get the CA.
 
Thanks & Regards,
 
K. Babu
 
----- Original Message -----
From: asad azmi
Sent: Tuesday, April 26, 2011 1:17 PM
Subject: Re: [MW:10852] acceptance standards for pittings for SA 516 GR 70 Plates

Dear mr. Babu,
 
construction code is ASME SEC VIII DIV 1.
 
Pittings were observed  on the plates during material receiving inspection.
 
pls inform me what is CA.
 
thanks and regards

On Tue, Apr 26, 2011 at 4:10 AM, Kathalingam Babu <kathalingam.qaqc@ppl.com.sg> wrote:
Hi Azad,
 
You can consider the CA, as allowable depth of pitting allowed for the respective grade.
 
What is the construction code ?
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
From: asad azmi
Sent: Monday, April 25, 2011 8:06 PM
Subject: [MW:10842] acceptance standards for pittings for SA 516 GR 70 Plates

Dear All,
 
Greetings.
 
what is the acceptance standard for pittings on SA 516 GR 70 Plate.
 
I mean what is the depth and diameter allowed.
 
Thanks and Regards
 
Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...