Re: [MW:10872] RE: Inconel 625 overlay on AISI4140

For Overlay weld ,Only corrosion properties are checked and not any other mechanical test .All mechanical properties are calculated on base metal of the component
Regards
Hegde P.b.


From: ravi <akravi54@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tue, 26 April, 2011 2:33:19 PM
Subject: Re: [MW:10859] RE: Inconel 625 overlay on AISI4140

Dear Mr Moturu,
 
How are you checking the effect of cyclic loads on the overlay? What kind of testing was carried out?
Regards,
Ravi
On Mon, Apr 25, 2011 at 1:43 PM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

What is you code of construction, was there any lethal or sour service requirements? Hardness restrictions? Requirement of SCC etc.

What is the tempering temperature of the base material (probably 540 °C is recommended as it should not exceed the tempering temperature), refer the datasheet tempering temperature for this material in the range of 540-680°C

 

From: venu moturu [mailto:moturuvenu@yahoo.com]
Sent: Sunday, April 24, 2011 10:57 AM
To: materials-welding@googlegroups.com
Cc: Bathula Raghuram (Mumbai - PIPING)
Subject: Inconel 625 overlay on AISI4140

 

Dear Friends,

 

Could anyone  pl. advice or guide us  as we wanted to weld corrosion resistant overlay of Inconel 625 on AISI 4140 on a used sub sea equipment in the oil and gas sector , where in the application demands severe Tensile and cyclic loads  on the component . The overlay shall be of approximately 4~5mm on a 100 mm thick section .

 

The vendor has submitted us two procedures with pulsed GMAW (Auto ) welding process having with and without  PWHT . When we referred the procedure with PWHT  we found that  the procedure is qualified (at  540 degreeC @ soaking time 2hrs and rate of heating 150 degree C/Hr)

 

can anyone help me out to send the literature with and without PWHT

 

Best regards

venu

 

 



 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...