Hi
 
As per my understanding, IZOD tests used to simulate the impact behaviour on the room temperature of Steels , Like aircraft body, Boiler applications
 
Also, Izod will generally used for the Plastics
 
With Respect to Prem , question Toughness for the Casting/Plate cannot be generalised , which will be governed by complex factors, Like grain structure & Mfg Process etc.
 


 
On Thu, Apr 21, 2011 at 7:07 PM, Lossie, Bert <Bert.Lossie@kiwa.nl> wrote:
Manpeet,
 
Izod is for plastics, charpy V notch ductility tesying is common on steels.
 

Kind regards

Met vriendelijke groeten,
Namens Kiwa N.V.

Ing. L. Lossie
IWE / I&K III
Senior inspecteur

Fax: (+31) 070-414 4420
Mobiel: (+31) 06-51615714
Email: bert.lossie@kiwa.nl

Subject: RE: [MW:10767] Impact testing temp. for EN19 steel

Hello !

 

Please can someone answer my general query>

 

Why only Charpy V Notch Testing is mostly used for Impact Testing & why Izod is not  popular.

 

Please give detailed information to understand process thoroughly.

 

Waiting for replies!

 

Regards,
Manmeet Magdum
Document Quality Control Drilling Riser Systems
QS Supply Chain.
AkerSolutions

( (Tel ) +91-20-66918751

Ë (Mobile) +91 9762446730
* (Email) Magdum.Manmmet@akersolutions.com

Aker Powergas Subsea   Pvt Ltd
BlueRidge , IT-2, Flagship Infrastructure Pvt Ltd, Ist Floor, Hinjewadi, Pune 411045, India

Registered in India ; CIN;U74990MH2010PTC210736

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu
Sent: Thursday, April 21, 2011 5:47 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10765] Impact testing temp. for EN19 steel

 

Hi

 

Izod will be done at Room temp.,  Unless  otherwise specifically mentioned by spec.

 

Thanks & Regards,

 

K. Babu

----- Original Message -----

Sent: Wednesday, April 20, 2011 11:21 PM

Subject: [MW:10758] Impact testing temp. for EN19 steel

 

Dear Friends

I wanted to use EN 19 plate in one of my present project, wherein the application demands severe impact loads at room temperature.

I had browsed through the properties of EN 19 plate in various literatures wherein the Izod test values are mentioned @ 55J.

However the Izod testing temperature is not mentioned.

Can anyone help me out or guide me where to refer, so that i can know the Izod testing temperature of this EN 19 steel.

Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?
The reason being the final component will have to be casted due geometrical complications.


Regards

Prem Nautiyal


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & regards,

K.Babu
Singapore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...