Skip to main content

Re: [MW:10540] Welder Qualification by UT

Dear Ramesh,
 
Find attached the file with description regarding the latest edition 2010 changes.
& also to qualify welders by UT in addition to the below points, a approved procedure for the same should be available.
 

Regards,

Yusufkhan. M. Pathan

Engineer-Quality

Air Liquide Engg (IND) Pvt.Ltd.

Cell:(+91) 8008804165


On Thu, Mar 31, 2011 at 9:16 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

Yes it is permitted from year 2010 edition (If you are asking for ASME BPV Sec IX).

Generally where the term "radiography" or its derivatives have been used in Section IX in the past, the phrase "or ultrasonic examination" has been added

or "volumetric NDE" is used. The acceptance criteria are similar to those for radiography. The big limit on using ultrasonic examination on performance qualification tests, however, is that the coupon or production weld must be ½ inch thick or thicker.

Forms QW-484A and QW-484B have been revised to add a check box choice of RT or UT when volumetric NDE is performed.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eng/ Mostafa Kamel Hussein
Sent: Thursday, March 31, 2011 1:24 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:10531] Welder Qualification

 

ِِAccording to ASME IX you have two options

1- By RT

2- By DT

No other option is permitted


From: Ramesh Barot <rameshnbarot@yahoo.com>
To: Materials Welding <materials-welding@googlegroups.com>
Sent: Wed, March 30, 2011 2:58:06 PM
Subject: [MW:10529] Welder Qualification

Dear all experts,

 

Can we qualify welder by UT?


 

Thanks,
With Best Regards,
Ramesh Barot


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...