Tuesday, February 8, 2011

Re: [MW:9766] HEAT AFFECTED ZONE CALCULATION

Dear Antony,
 
What do you mean from HAZ calculation? are you trying to calculate the width of HAZ?
 
There is no such direct calculation or ready made formula available to calculate the width of HAZ, generally the width of HAZ depends on several factors.
 
- Welding Process used,
- Welding parameters / Heat input used,
- Preheat / Interpass temperatures,
- Material and Thickness used, etc.,
 
 
Hope this helps,
 
Regards,
 
A.Praveen
Muscat
 
 
 
If you wanted to calculate the exact width, then weld a coupon and send it your lab for macro examination, after you etch the polished specimen you'll be able to clearly see the width of the HAZ.
 

--- On Mon, 2/7/11, antony jenis <antonyjenis@gmail.com> wrote:

From: antony jenis <antonyjenis@gmail.com>
Subject: [MW:9762] HEAT AFFECTED ZONE CALCULATION
To: materials-welding@googlegroups.com
Date: Monday, February 7, 2011, 7:48 PM

DEAR SIRS,

i need to calculate the heat affected zone for the 50 mm thickness plate as per AWS D1.1.
if you have any other code for the formula .


regards
antony jenis

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...