Hi Doug,
 
To the best of my knowledge SB-337 is more in ASME Sec-IX code from 2001 onwards. ASME Sec-II, deleted this material from the approved material list and also ASTM withdrew this material and replaced the same with B862(see attached).
 
As you know welding  Titanium requires extreme care and as  you have an existing qualified procedure on Titanium im place and I would think the following would be prudent:-
  • Do a thread bare comparison of both the specifications (B-337 & B862) and find their equivalence.
  • Should any equivalence be established, then it would be appropriate to put up a request with your local jurisdiction/ inspection agency concerned.
It the above is not possible, it would be wise to qualify a new procedure.
 
Note : Titanium group is 51,52,53, each group is not the same , there're numerous alloys approved by ASME Sec-IX. Thus the qualification should be within the same P No.
 
Thanks.
 
Pradip Goswami,P.Eng.IWE
Welding & Metallurgical Specialist & Consultant
Ontario, Canada.
Email-pgoswami@sympatico.ca,
 
 
 From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Doug McCasland
Sent: Monday, February 07, 2011 11:51 AM
To: materials-welding@googlegroups.com
Subject: [MW:9758] Titanium procedure

Need help ,
I have in place, a procedure to weld titanium using, P51 to P51 base metals(B-337 GR2) and  ERTI-1 filler metal. I need to be procedurally qualified to weld B862-05 GR2 material.
If the one I have is not sufficient, please advise me on what I need to do.

-- Thanks --

DOUG MCCASLAND
IDC SITE QA/QC
PH: 225-317-2889

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...