Hi Rems,
 
Ya its qualified, if the welder is qualified without backing, he can able to weld with & without backing. If he is qualified in with backing he cant weld without backing.
 
Regards,
 
E.S.Mani.

On Sat, Feb 5, 2011 at 10:43 AM, <lordrems@gmail.com> wrote:
According to ASME sec IX, change in P-number and F-number is an essential variable for welding performance qualification. QW-423 said that when a base metal with P- or S-No 1 through P- or S-No. 11, etc is used for welder qualification, the welder is qualified to weld all combinations of base metal with P- or S-No 1 thru P- or S-No 11 etc.
I have welders who are qualified on GTAW process using a P1 materials of course with F6 consumable, are these welders qualified to weld an Austenitic Stainless Steel (P8 material) with stainless steel consumable which is still under F6 with argon as the backing gas.

Regards
Rems Okonkwo
Nigerdock Nig PLC
Sent from my BlackBerry wireless device from MTN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--

Regards,

E.Subramanian


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...