Need help ,
I have in place, a procedure to weld titanium using, P51 to P51 base metals(B-337 GR2) and  ERTI-1 filler metal. I need to be procedurally qualified to weld B862-05 GR2 material.
If the one I have is not sufficient, please advise me on what I need to do.

-- Thanks --

DOUG MCCASLAND
IDC SITE QA/QC
PH: 225-317-2889

--