Re: Re: [MW:8851] interpass temperature- 13 Chrome Martensitic stainless steel

I recollect we had used E309L consumables and without PWHT.

Regards

Prem Nautiyal

On Tue, 21 Dec 2010 13:46:54 +0530 wrote
>Dear Prem
Can u pls tell me which consumable have you used for 13Cr martensitic stainless steel?I have also been told the sometimes duplex stainless steel consumables are used if more corrosion resistance is required. (ER 2594), but I am not sure of this fact.

Best regards


On Mon, Dec 20, 2010 at 6:08 PM, PREM SHANKARDUTT NAUTIYAL wrote:

Hi



You can Use interpass temp. of 250 degrees C. This is as per past experience and consumable manufacturer recommendations.



Prem Nautiyal





On Mon, 20 Dec 2010 08:27:46 +0530 wrote

>Dear All

What would be the maximum interpass temperature for 13 Chrome martensitic stainless steels?Is there any guideline for the same from any standard?





best regards











--

>

To post to this group, send email to materials-welding@googlegroups.com

>

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

>

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

>

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

>



PREM S NAUTIYAL

CELL : 9769316004





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...