Re: [MW:8806] Difference between E-7016 & E-7018

the main difference is iron powder in the coating for 7018. both electrodes are low hydrogen potassium type.
vanchi

On Sat, Dec 18, 2010 at 5:26 PM, pradip kumar sil <pradipsil@gmail.com> wrote:
Dear sir,
What is the quality wise difference between E-7018 ( BASIC LOW HYDROGEN) & E-7016 ( BASIC SODIUM LOW HYDROGEN).Can i use E-7018 insted of E-7016.
Where is the specific area of these two electrode
regards
sil

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...